So I'm in the middle of curing fires - did roughly 150, 200, 250, 300, 350, and tonight 400 degrees, each for about 4 hours. I'd like to put down lathe and stucco a scratch coat on the dome. Can I stucco before I do the last 450 and 500 degree curing fires? (If I get in a coat tomorrow, I can finish before temps dip below 40 at night.)
Also, how long do I have to let the scratch coat dry before the brown (second) coat?
Finally, I tried using metal cloth, but it was hard to smooth out the ridges (running top to bottom) due to the stiffness. I imagine chicken wire is more shape-able. Any reason not to use it? Or is it better to have the tighter weave of the metal cloth?
Also, how long do I have to let the scratch coat dry before the brown (second) coat?
Finally, I tried using metal cloth, but it was hard to smooth out the ridges (running top to bottom) due to the stiffness. I imagine chicken wire is more shape-able. Any reason not to use it? Or is it better to have the tighter weave of the metal cloth?