Hi,
Well into my build and near finishing.
I have 2 x layers that make 50mm of perlite render, 5 perlite, 1 lime, 1 plastering sand and 1 cement.
In the UK its hard to get silicone fine particle perlite so the particle size is up to 5mm. I am tiling the dome so i would like to give it one more coat that's smoother. What would be my best mix for this?
I did think about floor levelling compund mixed so its more workable and not so runny on the dome, but I'm really unsure? Maybe a final 6:1:1 sand, cement and lime mix?
Any past experience and advice would be greatly appreciated.
Chris
Well into my build and near finishing.
I have 2 x layers that make 50mm of perlite render, 5 perlite, 1 lime, 1 plastering sand and 1 cement.
In the UK its hard to get silicone fine particle perlite so the particle size is up to 5mm. I am tiling the dome so i would like to give it one more coat that's smoother. What would be my best mix for this?
I did think about floor levelling compund mixed so its more workable and not so runny on the dome, but I'm really unsure? Maybe a final 6:1:1 sand, cement and lime mix?
Any past experience and advice would be greatly appreciated.
Chris
Comment